Default Powder coating

I have a oven that can take 25 feet horizontal, 12 feet wide, and 12 feet tall. I have powdered small boat masts and booms, big boat booms and so many spin poles I can't even remember. With some of the new powder formulations out there (they look like chrome) we have even done winch drums complete with "alligator skin" effects. The techniques for powder are very similar to the Awlgrip methodolgies of high-build primers and color coats/seal coats, then gloss coats.
Metered correctly, powder and its base primer coat will fill most imperfections flawlessly.
There is one important thing to remember though. If the material is heavily oxidised there is the possibilty of an effect called "gassing" where the oxides reach critical mass and revert back to gassing causing tiny pin holes in the powder. We have turned away certain jobs because the oxidation is that bad. Sand blasting is not a viable option because the blast media will drive the oxidation further into the material to be coated. We have had great success with a hot bath of de-ionized water (think of a long jacuzzi). As with all finish jobs, proper preparation is 2/3 of the finished product.
Hope this helps.
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is On


All times are GMT -7. The time now is 05:07 PM.


Powered by vBulletin® Version 3.6.7
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.