Search: Posts Made By: Douglas
Forum: SparTalk 04-18-2015, 04:06 PM
Replies: 3
Views: 2,613
Posted By Douglas
Ring

Someone once told me that a useable bronze fitting will be one that has a clear ring when tapped with a hammer and suspended with a wire ,,,,, thus a cracked bronze fitting will sound a "thud"...
Forum: SparTalk 03-07-2015, 08:20 AM
Replies: 3
Views: 2,304
Posted By Douglas
Cloning Errors

Ahoy Brion , wondering what would be "Cloning Errors" on mast tangs ?

Do you suggest by this , that the tang displayed in the Benjiwood photo needs a nudge more shoulder area around the pin hole...
Forum: SparTalk 02-19-2015, 07:01 AM
Replies: 13
Views: 10,832
Posted By Douglas
Rubber Mast Wedges

Ahoy Brion ,,, do you stock or order those rubber wedges for mast to partner spaces ?
Forum: SparTalk 02-18-2015, 09:43 AM
Replies: 9
Views: 5,921
Posted By Douglas
FWIW Gleb , of greater concern might be the...

FWIW Gleb , of greater concern might be the surveyor's creed to never hang a structural fitting on a welded joint and what about the rusting corrosion under that Tee toggle ? :(
Forum: SparTalk 11-24-2014, 07:07 AM
Replies: 5
Views: 3,233
Posted By Douglas
aluminum corrosion

Heat has usually worked for me , Thanks Brion .

Wondering if anyone has used caustic soda (Lye n water) to remove those aluminum corrosion bubbles under paint ?
Forum: SparTalk 10-15-2014, 08:25 AM
Replies: 12
Views: 5,488
Posted By Douglas
Welding on Aluminum Spars

Ahoy bm , my Forespar mast fabricated around 1985 has spreader bases welded right to the mast wall .

FWIW , author Nigel Calder says this , in his second edition of Boatowner's Mechanical and...
Forum: SparTalk 10-15-2014, 08:03 AM
Replies: 3
Views: 2,782
Posted By Douglas
Potting S S

I concur with Brion's wise words of wisdom .

Some books that I have read in the past , say to "never" pot SS especially when used in or around salt water .

This holds true with fiberglass rudders...
Forum: SparTalk 10-05-2014, 11:04 AM
Replies: 2
Views: 2,638
Posted By Douglas
316 vs 304

Ahoy Calypso , Good Question on 1 X 19 SS rigging wire choices .

Back in circa 1980's Brion gave a one night talk on rigging and rig failures , at the Santa Cruz West Marine store .

His...
Forum: SparTalk 08-17-2014, 03:24 PM
Replies: 10
Views: 9,298
Posted By Douglas
954 is copper based alloy

That McMaster-Carr link , shows a copper based alloy (954) flanged bushing .

Without a pic , I am not quite sure of your application .

Riggers in the sailboat aluminum mast industry don't mate...
Forum: SparTalk 07-22-2014, 10:36 AM
Replies: 2
Views: 2,756
Posted By Douglas
Foil Sections

Maybe you can , "Think outside the box" , and cut them where needed then re-splice them .
Other methods might use heat to help break the bond .

I am wondering if caustic soda might help ?

...
Forum: SparTalk 06-12-2014, 08:52 PM
Replies: 1
Views: 2,182
Posted By Douglas
Rigging Standards

Sorry that I don't know of a specific "Rigging Standards" book for sailboats , but some of us boat owners use Nigel Calder's , book , "Boat Owners Mechanical and Electrical Manual" , for rigging...
Forum: SparTalk 06-03-2014, 06:19 AM
Replies: 1
Views: 2,189
Posted By Douglas
Butt Welding Mast Extrusions

Ahoy All , I had a forespar aluminium mast, that developed corrosion bubbling under the paint.
This occurred about 5 1/2' up from the bottom end of the mast , seen inside the cabin, as the mast is...
Forum: SparTalk 02-19-2014, 01:29 AM
Replies: 6
Views: 4,470
Posted By Douglas
Blue Metals

Gee , Storm , I am just a sailor who did the type of research that you are doing today.

It was explained to me that some of the Asian SS mills would skimp on Chrome or Nickel , if the prices were...
Forum: SparTalk 02-14-2014, 02:21 AM
Replies: 6
Views: 4,470
Posted By Douglas
Chainplate Material

Gee Whiz , Storm ,,, you will not find an answer to your question , better than Brion's .

Knowing that Gold is the best alloy to cap teeth ,,, how many people choose that expensive option ?

So we...
Forum: SparTalk 01-17-2014, 03:20 PM
Replies: 6
Views: 3,904
Posted By Douglas
Sealing Swages

Gosh , wouldn't we all like to have successful seals against stagnant salt water accumulating in the swage fittings ???

Marine surveyors say to just replace the SS wire and terminals at 10 year...
Forum: SparTalk 01-17-2014, 02:53 PM
Replies: 1
Views: 2,131
Posted By Douglas
Bronze Turnbuckles

I am glad we can still find some available , and I chose "Jaw" ends , used with eye Sta-Locs on the wire , so that I could change the wire end to end , when the lower end showed signs of rust...
Forum: SparTalk 01-05-2014, 06:52 PM
Replies: 1
Views: 2,235
Posted By Douglas
Eye vs T

There are many things to consider when making a choice like this , but structural strength comparison may not be a big one.

I would think that durability and long life may be more important ,...
Forum: SparTalk 01-05-2014, 06:30 PM
Replies: 2
Views: 2,452
Posted By Douglas
Bronze Chainplates

Ahoy ,,,, their should be a heap of info on this subject in the Spar Talk archives , for you to read.

L & L , cast aluminium nickel bronze for their Hess Cutter Seraffyn .

I have used silicon...
Forum: SparTalk 10-30-2013, 06:43 AM
Replies: 13
Views: 12,068
Posted By Douglas
Mast Tangs

Gulp ! that's a heap of information you are after ,,, but all of it, is important information .

Both Brion and Joe's answers on this forum have helped me heaps , in the past .

Maybe you would...
Forum: SparTalk 10-04-2013, 08:06 PM
Replies: 13
Views: 12,068
Posted By Douglas
Tee Strap Toggles

Ahoy ,,, all the recommendations for designing with SS structural fittings , that I have read about , is to never hang anything structural from a SS welded fitting , and that ALL ss structural...
Forum: SparTalk 09-29-2013, 05:16 PM
Replies: 13
Views: 12,068
Posted By Douglas
toggle design

Ahoy All ,,,, I am curious as to how the "Tee" on the tee-bolt stud toggle is formed ,,,, does anyone have a clue ?

Also has anyone put their 50 power h/h Edmund Scientific microscope on the bent...
Forum: SparTalk 09-26-2013, 08:42 AM
Replies: 1
Views: 2,536
Posted By Douglas
South Coast Blocks

Ahoy All ,,,, does anyone know what that red rubber is , that South Coast Block cheeks were made of ?
Forum: SparTalk 09-26-2013, 05:13 AM
Replies: 13
Views: 12,068
Posted By Douglas
Strap Toggles

Ahoy Mat ,,,, F W I W ,,,, I don't like ss strap toggles . My used boat came with SS strap toggles on the SS chain plates . The SS strap toggles were clean and bright, no rust showing .

Upon...
Forum: SparTalk 08-28-2013, 02:50 AM
Replies: 8
Views: 8,390
Posted By Douglas
Silicon Bronze

Ahoy Storm ,,, the last Silicon Bronze plate stock , that I purchased was from Alaskan Copper and Brass : http://www.alascop.com/pdf/brbr/silicon_comm_sheet.pdf ,,,,,, they shipped that small...
Forum: SparTalk 08-14-2013, 06:55 PM
Replies: 12
Views: 18,622
Posted By Douglas
Manganese C / P's

Ahoy Gary ,,, are you saying that your lower boomkin C / P's are made of Pete's Manganese castings ?

I guess if you are really concerned of de-zincification on long passages, you could add...