Quote:
Originally Posted by Russell
After a few months it started to get a bit brown, at the top of the swages and the screw ends.

Is this normal? I was hoping not to see rust for a long time.

Russell,

My bet would be that your gang was made up with 302/04 stainless vice 316. The 302/04 makeup is a little stronger than 316 but will discolor due to the higher carbon content and less nickel and chromium in 316.

Chances are your gang is fine. Just keep a watch at the terminal swages.